Research Output | Dar Al-hikmah Library | IIUM Only
Kenaf fiber (KF) based thermoplastic natural rubber (TPNR) composite was produced by melt blending with polypropylene (PP). Kenaf fiber (15% by volume) and TPNR were mixed in as Haake 600p internal mixer. The fracture behavior of the TPNR matrix and of TPNR–kenaf (with and without maleic anhydride grafted polypropylene, MAPP) composites was evalu