Hardening surface layer with and without adding reinforcing material can be achieved by rapid solidification on the top substrate area via high energy input fusion. In this work, the TIG torch heat input at 1344 J/mm is fused at 0.5 mm and 1.5 mm of working distances to incorporate the preplaced TiC particulates on the surface of AISI 4340 low allo